Mikrostrukturalna Degradacja
The mechanical properties and the microstructural degradation effect in an old low carbon steels after 100-years operating time
Grzegorz Lesiuk
,
Mieczysław Szata
,
Mirosław Bocian
Cite
DOI
Aspects of structural degradation in steels of old bridges by means of fatigue crack propagation
We present conclusions drawn from the studies related to old steel structures, especially those erected on the turn of the 19th …